Influence of Polymer Superplasticizers Usage on Workability and Compressive Strength of 30 MPa and 40 MPa Concrete
Abstract
The advancement of technology has provided various alternatives to address limitations in concrete construction. One effective method for enhancing the quality of concrete is by introducing additional materials, known as admixtures, during the concrete production phase. One such type of admixture that can significantly improve concrete quality is superplasticizer. The primary principle behind the use of superplasticizer is to create a repelling force between cement particles to prevent clumping, which can lead to the formation of air voids in the concrete. This, in turn, can reduce the strength or quality of the concrete. In this research, the focus will be on the use of concrete admixtures, specifically superplasticizer, to enhance concrete workability. One product of superplasticizer is Sika Viscocrete 3115 N, which will be used in this study. Superplasticizers like Sika Viscocrete 3115 N play a crucial role in improving the flow and workability of concrete mixes, making them easier to handle and place during construction. This leads to more efficient and high-quality concrete structures. The target compressive strengths are 30 MPa and 40 MPa with variations in the percentage of superplasticizer admixture usage at 0%, 0.25%, 0.5%, and 0.75%. The testing methods used to determine the workability value are the slump test and the slump flow test, while the compressive strength test is conducted using a compression testing machine at the Advanced Concrete Materials and Computational Mechanics Laboratory, Department of Civil Engineering, ITS. The study concludes that the addition of superplasticizer can enhance the workability of concrete but cannot optimally increase compressive strength. Additionally, different planned compressive strengths with the same percentage variation exhibit different trends. The addition of 0.25%-0.5% superplasticizer in both planned strengths still yields compressive strength above the planned levels, despite the decrease.
Keywords
Full Text:
PDFReferences
M. Ghosal, “Materials Today : Proceedings,” Mater. Today Proc., vol. 2, no. xxxx, 2023, doi: 10.1016/j.matpr.2023.07.196.
D. Batu and K. Tekan, “Pengaruh penambahan superplasticizer dan abu batu sebagai filler untuk meningkatkan kuat tekan beton normal,” vol. XIII, no. 1, pp. 10–17.
W. Beton, M. Tinggi, K. D. A. N. Kuat, and T. Beton, “Vol 4. No. 3 Juni 2016,” no. 629, pp. 107–113, 2002.
W. and Salmon, Reinforced Concrete Design. 1990.
G. Lokesh, P. N. Kumar, N. Aishwarya, P. Parthiban, and A. Ponshanmugakumar, “Materials Today : Proceedings Experimental study of the effect of water reducing admixtures on concrete,” Mater. Today Proc., no. xxxx, 2023, doi: 10.1016/j.matpr.2023.05.163.
R. Marpen and I. Permata, “Pembuatan Beton Self Compacting Concrete ( SCC ) dengan Variasi Pasir Lokal untuk Beton Precast Pada Bangunan Pelengkap Jalan,” vol. 10, no. 2, pp. 91–98, 2022.
F. Teknik, J. T. Sipil, U. Sam, and R. Manado, “Pengaruh variasi kadar superplasticizer terhadap nilai slump beton geopolymer,” pp. 283–291.
A. M. Olowofoyeku, O. M. Ofuyatan, J. Oluwafemi, A. Ajao, and O. David, “Effect of Superplasticizer on Workability and Properties of Self-Compacting Concrete,” J. Phys. Conf. Ser., vol. 1378, no. 4, 2019, doi: 10.1088/1742-6596/1378/4/042088.
D. P. Umum, “Spesifikasi bahan tambahan untuk beton departemen pekerjaan umum,” 1991.
R. Sitanggang, Novembri Swi Hutabarat, and Rahelina Ginting, “PENGGUNAAN SUPERPLASTICIZER PADA BETON MUTU F’c 25 MPa,” J. Ilm. Tek. SIPIL, vol. 11, no. 1, pp. 148–157, 2023.
A. Prasad, K. Sahoo, H. Sekhar, A. Pradhan, and B. Jena, “Materials Today : Proceedings Experimental study on the effect of superplasticizer on workability and strength characteristics of recycled coarse aggregate concrete,” Mater. Today Proc., vol. 60, pp. 488–493, 2022, doi: 10.1016/j.matpr.2022.01.324.
S. Pengajar, J. Teknik, S. Universitas, and K. Ternate, “Kusnadi , Dewi Sulistyorini,” vol. VII, no. 2, pp. 124–140, 2011.
A. Faqihuddin, Hermansyah, and E. Kurniati, “TINJAUAN CAMPURAN BETON NORMAL DENGAN PENGGUNAAN padat . Umumnya beton sudah banyak digunakan di berbagai jenis konstruksi , khususnya pada dibangun konstruksi , maka berkembanglah berbagai jenis beton menurut karakteristik dan,” vol. 2, no. 1, pp. 34–45, 2021.
G. Lai, X. Liu, S. Li, Y. Xu, Y. Zheng, and J. Guan, “Development of chemical admixtures for green and environmentally friendly concrete : A review,” J. Clean. Prod., vol. 389, no. January, p. 136116, 2023, doi: 10.1016/j.jclepro.2023.136116.
F. L. Y. Ash and D. A. N. Admixture, “Pengujian kuat tekan beton dengan penambahan fly ash dan admixture superplasticizer compressive strenght test of concrete added with fly ash and superplasticizer as a admixture,” vol. VII, no. 1, pp. 50–55, 2015.
V. B. Slat, S. W. M. Supit, N. Kondoj, J. Teknik, S. Politeknik, and N. Manado, “PENGARUH SUPERPLASTICIZER POLYMER TERHADAP,” 2003.
N. D. Shaikh, N. D. Shah, and F. Ash, “Materials Today : Proceedings Advancements in self-compacting geopolymer concrete : A comprehensive overview,” Mater. Today Proc., no. September, 2023, doi: 10.1016/j.matpr.2023.10.004.
D. Tjitradi, “NILAI SLUMP IDEAL UNTUK PERENCANAAN CAMPURAN BETON MUTU 50 Mpa,” vol. 13, no. 2, pp. 1–10, 2005.
K. Pustaka, “PENERAPAN SELF COMPACTING CONCRETE ( SCC ) PADA BETON MUTU NORMAL Oleh : Yogie Risdianto *),” vol. 08, pp. 54–60, 2010.
D. Pertiwi, T. Mca, and A. W. Setiawan, “The Use of Polymer Admixtures for Concrete Quality 45 Mpa Using the Combination of Bangkalan and Pandan Aggregate,” vol. 1, no. 2, pp. 89–98, 2022.
DOI: https://doi.org/10.31284/j.iptek.2024.v28i1.5283
Refbacks
- There are currently no refbacks.